Reaction Between High Mn-High Al Steel and CaO-SiO2-Type Molten Mold Flux: Retardation of Al2O3 Accumulation at High Al Content ([pct Al]0≥ 5) in Steel and Low MgO Content ((pct MgO)0≤ 1.8) in Flux.
Saved in:
| Title: | Reaction Between High Mn-High Al Steel and CaO-SiO2-Type Molten Mold Flux: Retardation of Al2O3 Accumulation at High Al Content ([pct Al]0≥ 5) in Steel and Low MgO Content ((pct MgO)0≤ 1.8) in Flux. |
|---|---|
| Authors: | Kim, Min-Su1, Park, Min-Seok2, Jung, Sung-Hoon2, Kim, Seong-Yeon3, Kang, Youn-Bae4, ybkang@postech.ac.kr |
| Source: | Metallurgical & Materials Transactions. Part B; 2020, Vol. 51 Issue 6, p3067-3078, 12p |