Enhancing the Selective Reduction of Nickel to Prepare FeNi50 Alloy from Saprolite-Type Laterite by CO-CO 2 Gas Pretreatment.
Saved in:
| Title: | Enhancing the Selective Reduction of Nickel to Prepare FeNi50 Alloy from Saprolite-Type Laterite by CO-CO 2 Gas Pretreatment. |
|---|---|
| Authors: | Hu, Zhichao1, Xue, Zhengliang1,2, xuezhengliang@wust.edu.cn, Hang, Guihua2,3, Lin, Guo1,3, Wang, Wei1,2, Huang, Fang1,3, Wang, Yaqi1 |
| Source: | Metals (2075-4701); Feb2026, Vol. 16 Issue 2, p236, 17p |
| Database: | Applied Science & Technology Source |
|