Retardation of the dewetting process due to the addition of functional copolymers at polymer–polymer interfaces.

Saved in:
Bibliographic Details
Title: Retardation of the dewetting process due to the addition of functional copolymers at polymer–polymer interfaces.
Authors: Wunnicke, O., Lorenz-Haas, C., Müller-Buschbaum, P., Leiner, V., Stamm, M.
Source: Applied Physics A: Materials Science & Processing. Dec2002 Supplement, Vol. 74 Issue 6, ps445. 1p.
Subjects: Copolymers, Polymers, Polystyrene, Polyamides
Abstract: We studied the retardation of the dewetting process due to the addition of a functional copolymer in a polymer bilayer film. The model system consists of fully deuterated polystyrene (PS-d) on top of an amorphous polyamide (PA) sublayer on silicon substrates. Bilayer films were prepared with different content (0, 5, 10 and 30 vol. %) of a statistical copolymer (protonated styrene maleic anhydride acid (SMA2) containing 2% MA groups along the chain) being capable of forming hydrogen bonds with PA. The asprepared as well as the annealed samples were investigated by neutron-reflectivity (NR) experiments, scanning force microscopy and optical microscopy. A significant retardation of dewetting is observed with the addition of SMA2. From model fits of NR curves the scattering length density profiles perpendicular to the sample surface were determined and an enrichment layer of SMA2 is detected. Retardation is explained by the intermixing of SMA2 and PS-d at the interface. [ABSTRACT FROM AUTHOR]
Copyright of Applied Physics A: Materials Science & Processing is the property of Springer Nature and its content may not be copied or emailed to multiple sites without the copyright holder's express written permission. Additionally, content may not be used with any artificial intelligence tools or machine learning technologies. However, users may print, download, or email articles for individual use. This abstract may be abridged. No warranty is given about the accuracy of the copy. Users should refer to the original published version of the material for the full abstract. (Copyright applies to all Abstracts.)
Database: Engineering Source
FullText Links:
  – Type: pdflink
Text:
  Availability: 0
Header DbId: egs
DbLabel: Engineering Source
An: 8905170
AccessLevel: 6
PubType: Academic Journal
PubTypeId: academicJournal
PreciseRelevancyScore: 0
IllustrationInfo
Items – Name: Title
  Label: Title
  Group: Ti
  Data: Retardation of the dewetting process due to the addition of functional copolymers at polymer–polymer interfaces.
– Name: Author
  Label: Authors
  Group: Au
  Data: <searchLink fieldCode="AR" term="%22Wunnicke%2C+O%2E%22">Wunnicke, O.</searchLink><br /><searchLink fieldCode="AR" term="%22Lorenz-Haas%2C+C%2E%22">Lorenz-Haas, C.</searchLink><br /><searchLink fieldCode="AR" term="%22Müller-Buschbaum%2C+P%2E%22">Müller-Buschbaum, P.</searchLink><br /><searchLink fieldCode="AR" term="%22Leiner%2C+V%2E%22">Leiner, V.</searchLink><br /><searchLink fieldCode="AR" term="%22Stamm%2C+M%2E%22">Stamm, M.</searchLink>
– Name: TitleSource
  Label: Source
  Group: Src
  Data: <searchLink fieldCode="JN" term="%22Applied+Physics+A%3A+Materials+Science+%26+Processing%22">Applied Physics A: Materials Science & Processing</searchLink>. Dec2002 Supplement, Vol. 74 Issue 6, ps445. 1p.
– Name: Subject
  Label: Subjects
  Group: Su
  Data: <searchLink fieldCode="DE" term="%22Copolymers%22">Copolymers</searchLink><br /><searchLink fieldCode="DE" term="%22Polymers%22">Polymers</searchLink><br /><searchLink fieldCode="DE" term="%22Polystyrene%22">Polystyrene</searchLink><br /><searchLink fieldCode="DE" term="%22Polyamides%22">Polyamides</searchLink>
– Name: Abstract
  Label: Abstract
  Group: Ab
  Data: We studied the retardation of the dewetting process due to the addition of a functional copolymer in a polymer bilayer film. The model system consists of fully deuterated polystyrene (PS-d) on top of an amorphous polyamide (PA) sublayer on silicon substrates. Bilayer films were prepared with different content (0, 5, 10 and 30 vol. %) of a statistical copolymer (protonated styrene maleic anhydride acid (SMA2) containing 2% MA groups along the chain) being capable of forming hydrogen bonds with PA. The asprepared as well as the annealed samples were investigated by neutron-reflectivity (NR) experiments, scanning force microscopy and optical microscopy. A significant retardation of dewetting is observed with the addition of SMA2. From model fits of NR curves the scattering length density profiles perpendicular to the sample surface were determined and an enrichment layer of SMA2 is detected. Retardation is explained by the intermixing of SMA2 and PS-d at the interface. [ABSTRACT FROM AUTHOR]
– Name: AbstractSuppliedCopyright
  Label:
  Group: Ab
  Data: <i>Copyright of Applied Physics A: Materials Science & Processing is the property of Springer Nature and its content may not be copied or emailed to multiple sites without the copyright holder's express written permission. Additionally, content may not be used with any artificial intelligence tools or machine learning technologies. However, users may print, download, or email articles for individual use. This abstract may be abridged. No warranty is given about the accuracy of the copy. Users should refer to the original published version of the material for the full abstract.</i> (Copyright applies to all Abstracts.)
PLink https://search.ebscohost.com/login.aspx?direct=true&site=eds-live&db=egs&AN=8905170
RecordInfo BibRecord:
  BibEntity:
    Identifiers:
      – Type: doi
        Value: 10.1007/s003390201856
    Languages:
      – Code: eng
        Text: English
    PhysicalDescription:
      Pagination:
        PageCount: 1
        StartPage: s445
    Subjects:
      – SubjectFull: Copolymers
        Type: general
      – SubjectFull: Polymers
        Type: general
      – SubjectFull: Polystyrene
        Type: general
      – SubjectFull: Polyamides
        Type: general
    Titles:
      – TitleFull: Retardation of the dewetting process due to the addition of functional copolymers at polymer–polymer interfaces.
        Type: main
  BibRelationships:
    HasContributorRelationships:
      – PersonEntity:
          Name:
            NameFull: Wunnicke, O.
      – PersonEntity:
          Name:
            NameFull: Lorenz-Haas, C.
      – PersonEntity:
          Name:
            NameFull: Müller-Buschbaum, P.
      – PersonEntity:
          Name:
            NameFull: Leiner, V.
      – PersonEntity:
          Name:
            NameFull: Stamm, M.
    IsPartOfRelationships:
      – BibEntity:
          Dates:
            – D: 02
              M: 06
              Text: Dec2002 Supplement
              Type: published
              Y: 2002
          Identifiers:
            – Type: issn-print
              Value: 09478396
          Numbering:
            – Type: volume
              Value: 74
            – Type: issue
              Value: 6
          Titles:
            – TitleFull: Applied Physics A: Materials Science & Processing
              Type: main
ResultId 1