CaO dissolution during melting and solidification of a Mg–10 wt.% CaO alloy detected with in situ synchrotron radiation diffraction.

Saved in:
Bibliographic Details
Title: CaO dissolution during melting and solidification of a Mg–10 wt.% CaO alloy detected with in situ synchrotron radiation diffraction.
Authors: Wiese, B.1 bjoern.wiese@hzg.de, Mendis, C.L.1, Tolnai, D.1, Stark, A.2, Schell, N.2, Reichel, H.-P.3, Brückner, R.3, Kainer, K.U.1, Hort, N.1
Source: Journal of Alloys & Compounds. Jan2015, Vol. 618, p64-66. 3p.
Subjects: Magnesium compounds, Lime (Minerals), Dissolution (Chemistry), Solidification, Synchrotron radiation, Temperature effect, Melting
Abstract: The phase dissolution and evolution during the melting and the solidification of Mg containing 10 wt.% CaO was investigated in the temperature range of 20–680 °C. The dissolution of CaO and the formation of Mg 2 Ca were detected with in situ synchrotron radiation diffraction. The dissolution of CaO was observed at ∼407 °C with the detection of a peak unique to the Mg 2 Ca phase prior to melting of Mg. After the solidification no CaO was detected, and Mg 2 Ca and MgO phases were observed. [ABSTRACT FROM AUTHOR]
Copyright of Journal of Alloys & Compounds is the property of Elsevier B.V. and its content may not be copied or emailed to multiple sites without the copyright holder's express written permission. Additionally, content may not be used with any artificial intelligence tools or machine learning technologies. However, users may print, download, or email articles for individual use. This abstract may be abridged. No warranty is given about the accuracy of the copy. Users should refer to the original published version of the material for the full abstract. (Copyright applies to all Abstracts.)