Compressive creep behaviour of Yb4Si2O7N2 containing silicon nitride ceramic between 1400 and 1500°C.
Saved in:
| Title: | Compressive creep behaviour of Yb4Si2O7N2 containing silicon nitride ceramic between 1400 and 1500°C. |
|---|---|
| Authors: | Guo, S., Hirosaki, N., Nishimura, T. |
| Source: | Materials Science & Technology; April 2003, Vol. 19 Issue 4, p544-548, 5p |
| Database: | Applied Science & Technology Source |
| ISSN: | 02670836 |
|---|---|
| DOI: | 10.1179/026708303225001911 |