Comparative Evaluation of Tear Strength of Two Platinum-Based Maxillofacial Silicone Materials: Siloczest LSR With and Without the Addition of 2.5% Zinc Oxide (ZnO) Nanoparticles and Technovent (m511)-An In Vitro Study.

Saved in:
Bibliographic Details
Title: Comparative Evaluation of Tear Strength of Two Platinum-Based Maxillofacial Silicone Materials: Siloczest LSR With and Without the Addition of 2.5% Zinc Oxide (ZnO) Nanoparticles and Technovent (m511)-An In Vitro Study.
Authors: Sharan S; Department of Prosthodontics Including Crown and Bridge, Dayananda Sagar College of Dental Sciences and Hospital, Bengaluru, India., Sarandha DL; Department of Prosthodontics Including Crown and Bridge, Dayananda Sagar College of Dental Sciences and Hospital, Bengaluru, India., Sujana S; Department of Prosthodontics Including Crown and Bridge, Dayananda Sagar College of Dental Sciences and Hospital, Bengaluru, India., Shah MA; Department of Public Health Dentistry, Government Dental College and Hospital, Jamnagar, Gujarat, India., Kamath V; Department of Prosthodontics Crown and Bridge, Manipal College of Dental Sciences Mangalore, Manipal Academy of Higher Education, Manipal, Karnataka, India.
Source: TheScientificWorldJournal [ScientificWorldJournal] 2025 Oct 17; Vol. 2025, pp. 3581428. Date of Electronic Publication: 2025 Oct 17 (Print Publication: 2025).
Publication Type: Journal Article; Comparative Study
Journal Info: Publisher: Wiley Country of Publication: United States NLM ID: 101131163 Publication Model: eCollection Cited Medium: Internet ISSN: 1537-744X (Electronic) Linking ISSN: 1537744X NLM ISO Abbreviation: ScientificWorldJournal Subsets: MEDLINE
Database: MEDLINE Ultimate
Full text is not displayed to guests.
Description
ISSN:1537-744X
DOI:10.1155/tswj/3581428